Visualize a published system sheet


FNP system
The substrate temperature, the relative humidity and the dry film thickness can significantly impact the drying times. Provide sufficient ventilation during application to facilitate water evaporation. At a humidity level higher than 60% and a temperature < +15°C, drying is greatly slowed down.

Codification:

Codifications published
PIA/EIA PIB/EIB PID/EID 154
PIA/EIA PIB/EIB PID/EID 152

Coat list

Coat number Product name Thickness Nature of the binder Type of phase Proportion of solvent
1 HYDROCENTRIFUGON PEINTURE NF IVORY RAL 1015 50 µm Epoxy-polyaminoamide AQ
2 HYDROCENTRIFUGON PEINTURE NF WHITE RAL 9010 50 µm Epoxy-polyaminoamide AQ